Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 744 MPa @Strain 0.200 % |
108000 psi @Strain 0.200 % |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 25% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |