Polymer Property : Tensile Strength, Yield = 735.5 MPa
Polymer Property :
Tensile Strength, Yield =
735.5 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
>=
735.5
MPa
>=
106700
psi
Crucible Steel 422 (JIS SUH616) Martensitic Steel
Information provided by Crucible Specialty Metals.