Polymer Property : Tensile Strength, Yield = 725 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.80 - 5.00 MPa
551 - 725 psi
Average value: 4.28 MPa Grade Count:9
Overview of materials for Styrenic TPE  (Unverified Data**)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe..