Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 487 MPa @Strain 0.200 % |
70600 psi @Strain 0.200 % |
statistical analysis gives AVG-3STD at 438 MPa |
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Extruded Bar Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part.. |
|||
Tensile Strength, Yield | 487 MPa @Treatment Temp. 871 °C, Time 1.44e+7 sec |
70600 psi @Treatment Temp. 1600 °F, Time 4000 hour |
0.2%. Room temp test after thermal exposure |
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened, after long term high temperature exposure Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |