Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.86 MPa | 1140 psi | ASTM D412 |
Teknor Apex APEX® 1700-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Met.. |
|||
Tensile Strength, Yield | 7.86 MPa | 1140 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SHM 6200 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 7.86 MPa | 1140 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SFW 10500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Uses: Footwear; General Purpose Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |