Polymer Property : Tensile Strength, Yield = 7.336 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.336 MPa
1064 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7045 Ethylene-Propylene Rubber
General service EPDM.Information provided by Seals Eastern, Inc.