Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.074 MPa | 1026 psi | @100% Elongation; ASTM D1414 |
Greene Tweed Fluoroelastomer 742 FKM Fluoroelastomer 742 performs well in aggressive chemicals and where ultrapure materials are not required. Recommended for conventional wet and dry system applications, Fluoroelastomer 742 has a goo.. |