Polymer Property : Tensile Strength, Yield = 6720 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.3 MPa
6720 psi
Ineos ABS Lustran® 488
Key Features:UnfilledSuitable processing methods:Injection molding