Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 46.21 MPa | 6702 psi | ASTM D638 |
Lucent Polymers GPP-110 Polypropylene Homopolymer, 10% Glass Fiber Reinforced, Chemically Coupled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |