Polymer Property : Tensile Strength, Yield = 67.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 67.8 MPa
9830 psi
ASTM D638
Nylene® PA6/6 Impact Modified 411 HS Nylon 6/6
Medium Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.