Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 4.36 MPa | >= 632 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7045 Ethylene-Propylene Rubber General service EPDM.Information provided by Seals Eastern, Inc. |