Mechanical Properties Metric English Comments
Tensile Strength, Yield 530 - 630 MPa

@Strain 0.200 %
76900 - 91400 psi

@Strain 0.200 %
CLAL-MSX SICLANIC S® TH3 Quenched Copper Alloy, 1/2 Hard, precipitation treated
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..