Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.434 MPa | 63.0 psi | ASTM D638 |
Lord Adhesives Thermosetâ„¢ UR-340 Two Component Urethane Encapsulant Lord UR-340 is a two component, room temperature curing, urethane encapsulating compound. It is low in viscosity and has excellent flow characteristics. Its flexibility, low modulus characteristics,.. |