Mechanical Properties Metric English Comments
Tensile Strength, Yield 625 MPa

@Strain 0.200 %
90600 psi

@Strain 0.200 %
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Yield 625 MPa

@Strain 0.200 %
90600 psi

@Strain 0.200 %
Haynes 214® alloy, 10% cold reduction, 980°C (1800°F) for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 625 MPa

@Strain 0.200 %
90600 psi

@Strain 0.200 %
Haynes 214® alloy, 50% cold reduction, 925°C for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 625 MPa

@Strain 0.200 %,
Temperature 705 °C
90600 psi

@Strain 0.200 %,
Temperature 1300 °F
Haynes 242® alloy, cold rolled sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Copyright © lookpolymers.com All Rights Reserved