Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.3 MPa

@Thickness 3.20 mm
9030 psi

@Thickness 0.126 in
10mm/min; ASTM D638
LG Chemical LUCEL N145LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical