Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.46 MPa | 937 psi | ASTM D412 |
Polymax® Maxelast® P3670 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 6.46 MPa | 937 psi | -15% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering N70U Nitrile Rubber Nitrile Butadiene Rubber (NBR) 65-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD458A Grade A1 (specification inactive for new design).Application.. |