Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.12 MPa | 888 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7182X Fluorocarbon-Elastomer Formulated AFLAS®. Ultra-low compressive stress relaxation for alkaline, high-temperature service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 6.12 MPa | 887 psi | 100% Secant; ASTM D638 |
Dow AFFINITY™ EG 8100G Ethylene-octene copolymer AFFINITY™ EG 8100G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene-octene copolymer exhibiting high flexibility and elasticity. It can be utilized.. |