Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 407 MPa @Temperature 21.1 °C |
59000 psi @Temperature 70.0 °F |
0° Direction, Wet; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Strength, Yield | 407 MPa @Strain 0.200 % |
59000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 407 MPa @Strain 0.200 % |
59000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 407 MPa @Strain 0.200 % |
59000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 407 - 462 MPa | 59000 - 67000 psi | 0.2% offset |
Eagle Brass 210 Gilding Metal, Spring CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Yield | 407 - 538 MPa | 59000 - 78000 psi | 0.2% offset |
Eagle Brass 725 Copper Nickel Tin, 1/2 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Strength, Yield | 407 - 503 MPa | 59000 - 73000 psi | 0.2% offset |
Eagle Brass 735 Nickel Silver 18%, 3/4 Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | 407 MPa @Strain 0.200 %, Temperature -73.0 °C |
59000 psi @Strain 0.200 %, Temperature -99.4 °F |
Transverse |
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | 407 MPa @Strain 0.200 % |
59000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 760°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |