Polymer Property : Tensile Strength, Yield = 59.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.2 MPa
8590 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers NPP 60-3301 Clear Polyester Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 59.2 MPa
8590 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers NPP 60-3302 Clear Polyester Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 59.2 MPa
8590 psi
ASTM D412
C.O.I.M. LARIPUR® LPR7015 Plasticized Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..