Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 396 MPa @Temperature 23.0 °C |
57400 psi @Temperature 73.4 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, Annealed (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Tensile Strength, Yield | 396 MPa @Strain 0.200 % |
57400 psi @Strain 0.200 % |
typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Annealed Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |