Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 571 MPa @Strain 0.200 % |
82800 psi @Strain 0.200 % |
|
ATI Allvac® 9310 UNS G93106, UNS H93100 Specialty Steel Uses: Automotive applications, structural components, gears, rods, heat-treatable shafts.Property values are for samples in the metallurgical condition: 1630°F normalized.Information provided by Al.. |