Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 57.8 MPa | 8390 psi | ASTM D638 |
Teknor Apex Sinvicomp SRF 9702/C Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Medium Impact Resistance Uses: Electrical/Electronic Applications Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |