Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 56.9 - 57.1 MPa | 8250 - 8280 psi | ASTM D638M |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Tensile Strength, Yield | 56.9 - 57.1 MPa | 8250 - 8280 psi | ASTM D638M |
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons.. |