Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.392 MPa | 56.9 psi | ASTM D412 |
Microcell Composite Company CELLAMP® M5010 Thermoplastic Foam CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high.. |
|||
Tensile Strength, Yield | 0.392 MPa | 56.9 psi | ASTM D412 |
Microcell Composite Company CELLAMP® M5110 Thermoplastic Foam CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high d.. |