Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 559 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 559 MPa
>= 81100 psi
Crucible Steel 21-4N (JIS SUH35) Martensitic Steel
Information provided by Crucible Specialty Metals.
Tensile Strength, Yield >= 559 MPa
>= 81100 psi
Crucible Steel 21-4NNb Martensitic Steel
Information provided by Crucible Specialty Metals.
Tensile Strength, Yield >= 559 MPa
>= 81100 psi
Crucible Steel 21-4NNbW Martensitic Steel
Information provided by Crucible Specialty Metals.
Tensile Strength, Yield >= 559 MPa
>= 81100 psi
Crucible Steel 214NS (JIS SUH36) Martensitic Steel
Information provided by Crucible Specialty Metals.
Copyright © lookpolymers.com All Rights Reserved