Polymer Property : Tensile Strength, Yield = 55.86 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.86 MPa
8102 psi
ASTM D638
Lucent Polymers PC/ABS-1218 Polycarbonate+ABS, Easy Flow, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.