Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.8 MPa
5480 psi
51 mm/min; ASTM D638
I. Stern 1320NA Prime Homopolymer Polypropylene
Features:Good flow characteristicsAntistat propertiesLow odorApplicationsThin wall packagingSmall appliancesAutomotiveInformation provided by I. Stern & Co. Inc.
Tensile Strength, Yield 37.8 MPa

@Temperature 23.0 °C
5480 psi

@Temperature 73.4 °F
Molded and tested under D410, 50 mm/min; ASTM D638
Ineos H11G-00 Polypropylene Homopolymer
This is a barefoot homopolymer designed for fiber applications.ApplicationsStaple FiberOriented YarnBenefitsConsistent processabilityInformation provided by Ineos Olefins & Polymers USA
Tensile Strength, Yield 37.8 MPa

@Temperature 23.0 °C
5480 psi

@Temperature 73.4 °F
ASTM D638
Ineos H20Z-03 Polypropylene Homopolymer
This is a homopolymer containing nucleation and antistatic. It is designed for injection molding and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520...