Polymer Property : Tensile Strength, Yield = 54700 psi
Polymer Property :
Tensile Strength, Yield =
54700 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
377
MPa
54700
psi
90º, RT, Dry; EN2561
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber
Information provided by HexCel