Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.1 MPa | 5380 psi | chs 20 in/min; 50% elongation; ASTM D412 |
Diamond Polymers Softflex® 1302 Thermoplastic Elastomer Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |