Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 483 - 531 MPa | 70000 - 77000 psi | 0.2% offset |
Eagle Brass 194 HSM® Copper, Extra Spring High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |