Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 364 MPa @Thickness 25.4 mm, Temperature 25.0 °C |
52800 psi @Thickness 1.00 in, Temperature 77.0 °F |
0.2% offset |
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Tensile Strength, Yield | 364 MPa @Strain 0.200 %, Temperature 20.0 °C |
52800 psi @Strain 0.200 %, Temperature 68.0 °F |
strip with ASTM grain size of 10.5-11.0 |
Special Metals INCOLOY® alloy 832 Stainless Steel INCOLOY® alloy 832 is a low cost stainless steel developed specifically for domestic and industrial sheathed heater applications. With specific chemistry additions to ensure satisfactory formula.. |
|||
Tensile Strength, Yield | 364 MPa @Strain 0.200 %, Thickness 0.500 mm |
52800 psi @Strain 0.200 %, Thickness 0.0197 in |
strip with ASTM grain size of 10.5-11.0 |
Special Metals INCOLOY® alloy 832 Stainless Steel INCOLOY® alloy 832 is a low cost stainless steel developed specifically for domestic and industrial sheathed heater applications. With specific chemistry additions to ensure satisfactory formula.. |
|||
Tensile Strength, Yield | 364 MPa @Strain 0.200 % |
52800 psi @Strain 0.200 % |
|
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Plate 0.500 in (12.7 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.500 inch plate. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |