Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 52.08 MPa | 7553 psi | ASTM D-638 |
Axiall ProTherm® 4303 Rigid PVC, Extrusion Georgia Gulf 4303 is a CPVC powder formulation designed for the processing of pipe products with an O.D. range of 1/2" to 8 inches requiring high heat deflection temperatures. Processing and stabil.. |