Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.96 - 35.2 MPa
1300 - 5110 psi
Average value: 25.1 MPa Grade Count:200
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..