Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 280 - 350 MPa @Strain 0.200 % |
40600 - 50800 psi @Strain 0.200 % |
|
SSAB Tunnplat Aluzink 280A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Tensile Strength, Yield | 280 - 350 MPa @Strain 0.200 % |
40600 - 50800 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 280YP High-strength Steel High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report.. |
|||
Tensile Strength, Yield | 280 - 350 MPa @Strain 0.200 % |
40600 - 50800 psi @Strain 0.200 % |
|
SSAB Tunnplat Dogal 280YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Tensile Strength, Yield | 250 - 350 MPa @Strain 0.200 % |
36300 - 50800 psi @Strain 0.200 % |
|
CLAL-MSX NICLAL 3444 H12 1/2 Hard Copper Alloy, Free Cutting Bronze Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b.. |