Polymer Property : Tensile Strength, Yield = 5040 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.7 MPa
5040 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® LH-0300 ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 34.7 MPa
5040 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® LH-0300 ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 34.7 MPa
5040 psi
2.0 in/min; ASTM D638
ExxonMobil PP4792E1 Polymer Grade for Oriented Film
Product Description: Easy processing grade primarily for oriented film applications.Availability: North America Features:MetalizableUses: Oriented FilmPackagingTapeProcessing Method: Film Extrusi..