Polymer Property : Tensile Strength, Yield = 50.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.6 MPa
7340 psi
Elastic Limit
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv..
Tensile Strength, Yield 50.6 MPa
7340 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers ABSPC 9901B ABS/PC Blow Molding Grade, High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 50.6 MPa
7340 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers ABSPC 9901B-50148 ABS/PC Blow Molding Grade, High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.