Polymer Property : Tensile Strength, Yield = 5.93 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.93 MPa
860 psi
ASTM D412
Teknor Apex Flexalloy® 9800-50 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MW Uses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and..
Tensile Strength, Yield 5.93 MPa
860 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® IT 38-034M Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDiscla..
Tensile Strength, Yield 5.93 MPa
860 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® IT38-034 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDi..
Tensile Strength, Yield 5.93 MPa
860 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-4060 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionInforma..