Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.59 MPa | 811 psi | -35% change after 336 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering F60R Fluorosilicone Rubber Red Fluorosilicone, 56-65 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 60.Applications: S.. |
|||
Tensile Strength, Yield | 5.59 MPa | 811 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® T370A Thermoplastic Polyurethane Type: Estane® T370A is a Shore 74A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |