Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.43 MPa
498 psi
Microcell Composite Company CELLOMER® 2100DR SBS Rubber Pellets
CELLOMER® PELLETS can be used in hot-pressing or with injection foaming boards. Featuring anti-slippage and elasticity.Information provided by Microcell Composite Company
Tensile Strength, Yield 3.43 MPa
498 psi
at 100% elongation; ASTM D412
Lubrizol Estane® S175A Thermoplastic Polyurethane
Type: Estane® S175A is a Shore 77A, polyester type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mid..