Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 493 MPa @Strain 0.200 % |
71500 psi @Strain 0.200 % |
|
Haynes Multimet® alloy, 533.4 by 82.55 mm forging, stress relieved at 649°C (1200°F), air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and i.. |