Mechanical Properties Metric English Comments
Tensile Strength, Yield 492 MPa

@Strain 0.200 %
71400 psi

@Strain 0.200 %
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..