Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 336 MPa @Temperature 204 °C |
48700 psi @Temperature 399 °F |
|
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |
|||
Tensile Strength, Yield | 336 MPa @Strain 0.200 %, Temperature 538 °C |
48700 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |