Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.36 MPa | 487 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-165 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.36 MPa | 487 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-165 Dow-Corning Class VI Elastomer Information provided by Multibase |