Polymer Property : Tensile Strength, Yield = 486 MPa
Polymer Property :
Tensile Strength, Yield =
486 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
486
MPa
70500
psi
CMW® 3970 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, OrdnanceInformation provided by CMW Inc.