Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 334 MPa @Strain 0.200 % |
48500 psi @Strain 0.200 % |
|
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 2.0 inch (51 mm) Diameter Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 2.0 inc.. |