Polymer Property : Tensile Strength, Yield = 48.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.7 MPa

@Temperature 23.0 °C
7060 psi

@Temperature 73.4 °F
ASTM D638
PolyOne Geon™ CPVC MC550 Polyvinyl Chloride, Chlorinated (CPVC)
Information provided by PolyOne
Tensile Strength, Yield 48.7 MPa
7060 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers ASAPC 6040 UV Stabilized
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.