Tensile Strength, Yield 47.40 MPa
6875 psi
chs 2 in/min; ASTM D638
Diamond Polymers ASA T-120
Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc.