Polymer Property : Tensile Strength, Yield = 46800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 323 MPa

@Strain 0.200 %
46800 psi

@Strain 0.200 %
Typical
ATI Allegheny Ludlum AL 610 Stainless Steel, UNS S30600
AL 610 alloys are low-carbon, silicon-containing, austenitic stainless steels. These alloys are typically used for applications in the chemical industry. The high silicon content provides them wit..
Tensile Strength, Yield 323 MPa

@Strain 0.200 %
46800 psi

@Strain 0.200 %
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 649°C (1200°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..