Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.22 MPa
467 psi
ASTM D412
Polymax® Maxelast® P1765A TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 3.22 MPa
467 psi
ASTM D412
Polymax® Maxelast® S4730 TPE, PS Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong ..