Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 46600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 321 MPa

@Strain 0.200 %,
Temperature 816 °C
46600 psi

@Strain 0.200 %,
Temperature 1500 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Tensile Strength, Yield 321 MPa

@Strain 0.200 %
46600 psi

@Strain 0.200 %
Haynes HR-160® alloy, annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Tensile Strength, Yield 321 MPa

@Strain 0.200 %
46600 psi

@Strain 0.200 %
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Tensile Strength, Yield 321 MPa

@Temperature 70.0 °C
46600 psi

@Temperature 158 °F
transverse
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-7 (UNS S20153)
AL 201LN™ is a special composition of Type 201 specifically for sub-zero temperature service as welded tanks and vessels. This alloy has replaced the familiar 300 series stainless such as type 301..
Tensile Strength, Yield 321 MPa
46600 psi
Typical
Materion AlBeMet® AM 162 Rolled Sheet, Annealed
Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are..